Document |
Document Title |
JP5841157B2 |
Disclosed is a heat-shrinkable polyester film having a heat shrinkage initiation temperature of 60°C or lower, a glass transition temperature (Tg) of 77°C or lower and a heat shrinkage rate of 2% or more at 60°C which has relatively l...
|
JP2015229242A |
To provide a heat-shrinkable polyester film having high vertical thermal shrinkage, exhibiting low horizontal thermal shrinkage, and having excellent shrink finishing properties.A heat-shrinkable polyester film which is made of polyester...
|
JP5832639B2 |
A device and a method for a field expansion. A support core (30) is inserted into the device by a field expansion apparatus. The field expansion apparatus has a pressure applying means (20) defining a radially expandable inner surface an...
|
JP2015174939A |
To provide a packaging film that is composed of a resin composition with a small amount of addition of plasticizer and is excellent in packaging machine suitability, gas barrier properties, and retort properties.A packaging film is compo...
|
JP5785990B2 |
We disclose a monovinylarene-conjugated diene block copolymer containing a plurality of monovinylarene-conjugated diene mixed blocks, wherein each mixed block contains conjugated diene units and monovinylarene units in a weight ratio of ...
|
JP5774231B2 |
A vehicle suspension thermally shrinkable tube of the present invention is formed in a shape corresponding to a vehicle-suspension coil spring having a spiral shape and is formed so as to have a larger diameter than the diameter of the s...
|
JP5770917B1 |
To form a fine plating pattern on a resin. A heat-shrinkable heat-shrinkable resin 110, a modified portion formed so that a plating film 140 is deposited on the surface of the heat-shrinkable resin 110, and a plating film 140 formed on t...
|
JP5771340B1 |
The present invention provides a heat recovery article that shrinks heat in an appropriate temperature range, generates less bloom and bleed, and has excellent copper damage resistance, and a wire splice and a wire harness using this hea...
|
JP2015145070A |
To provide a method of achieving a functional surface having a fine structure of 1 μm or less using simple plastic deformation and buckling.A structure comprises an elastic body, and a thin film formed on the surface of the elastic body...
|
JP5761281B2 |
|
JP5761282B2 |
|
JP5760160B2 |
|
JP3197440U |
To provide a spiral shrink tube for holding an electrode having a thin and wide area for a long time. A thin tape 6 of a film in which an adhesive is applied to one side of a vertically or horizontally stretched film is first wound aroun...
|
JP5722081B2 |
|
JP5709378B2 |
The invention relates to films and methods of making the same. The inventive films comprise at least three layers, an inner layer and at least two outer layers located at opposite surfaces of the inner layer. In one embodiment, the inner...
|
JP2015081351A |
To provide a phosphorus-containing thermoplastic polyester having flame retardancy suitable for production of a phosphorus-containing heat-shrinkable tube.A polyester has an intrinsic viscosity of 0.70-1.10 dL/g, contains a phosphorus-co...
|
JP5700920B2 |
|
JP2015063650A |
To provide a heat shrinkable film small in tensile elongation, excellent in low-temperature shrinkability and excellent even in appearance after shrinkage.The method for manufacturing a heat shrinkable polyethylene film comprises the ste...
|
JP5695829B2 |
To obtain a heat-shrinkable film which satisfies shrink finishability, is excellent in heat shrinkage properties, mechanical properties such as breaking resistance and impact resistance, and transparency and is suitable for purposes such...
|
JP5687866B2 |
|
JP5686601B2 |
Disclosed is a thermo-shrinkable polyester film in which shrinkage uniformity is ensured in a shrinking process thus realizing superior quality of the outer appearance without causing a poorly printed state, reducing the production cost ...
|
JP5682841B2 |
|
JP2015034061A |
To provide a package having a favorable tearing condition of a covered label formed of a heat shrinkable film.A package is formed by at least partially covering an outer periphery with a label which is formed of a heat shrinkable film as...
|
JP5660852B2 |
|
JP5637272B2 |
|
JP5636907B2 |
|
JP5633808B2 |
|
JP5629548B2 |
To provide a heat shrinkable tube compatibly satisfying excellent impact resistance and printing aptitude, and suitable for covering a secondary battery such as a lithium ion battery.The heat shrinkable tube includes a polyesteric resin ...
|
JP5604823B2 |
To provide a cavity-containing heat-shrinkable polyester-based film that has light beam cutting property and a desirable white appearance, that has an apparent density smaller than water, and that has small variance in the size of caviti...
|
JP5602861B2 |
A polyamide resin-based heat-shrinkable multilayer film having excellent heat shrinkability and strength, as well as a high degree of deep A polyamide resin-based heat-shrinkable multilayer film having excellent heat shrinkability and st...
|
JP5588366B2 |
|
JP5587136B2 |
|
JP5577602B2 |
|
JP5577601B2 |
|
JP5572961B2 |
|
JP5569385B2 |
|
JP5562453B2 |
To provide a method of manufacturing a foamable and heat-shrinkable multilayer film, capable of achieving high shrinkability and productivity when used in a shrink label for use in a heating container or the like, and superior in heat re...
|
JP5545627B2 |
|
JP5537351B2 |
To provide a polylactic acid heat-shrinkable film with superior breaking resistance in a longitudinal direction and a width direction of the polylactic acid heat-shrinkable film, having favorable transparency and low temperature shrinkag...
|
JP5487596B2 |
|
JP5476533B2 |
|
JP5481757B2 |
A mixture which comprises a) from 5 to 95% by weight of a copolymer A which comprises one or more copolymer blocks (B/S)A each composed of from 65 to 95% by weight of vinylaromatic monomers and from 35 to 5% by weight of dienes and of a ...
|
JP2014064963A |
To provide a super water-repellent basal plate that has regions having different water droplet adsorption.A super water-repellent basal plate is produced by a method that includes: a drawing process in which stress is added in an almost ...
|
JP5467391B2 |
Provided are a method and an apparatus for producing a heat-shrinkable tube. An apparatus 100 includes a pair of pinch rollers 105 that can be moved along a feeding path of a tube 101 and that can be opened and closed with the feeding pa...
|
JP5446058B2 |
|
JP5433804B1 |
[Task] Provided is a heat-shrinkable film having good shrinkage characteristics even when reheated after shrinkage packaging, excellent in mechanical properties and transparency, and suitable for applications such as shrinkage packaging,...
|
JP5424257B2 |
A film comprises a skin layer, a base layer, and an intermediate layer between the skin and base layers. The skin layer comprises polyester. The base layer comprises styrenic block copolymer having a styrene monomer content of at least a...
|
JP5416090B2 |
|
JP5408250B2 |
Disclosed is a heat shrinkable polyester film which does not suffer (namely natural shrinkage), is suppressed in decrease of the shrinkage in the main shrinkage direction, and is able to be beautifully and efficiently fitted to a contain...
|
JP5380830B2 |
To provide a heat shrinkable polyolefine film that is high in the shrinkability in the longitudinal direction being its main shrinkage direction, excelling in shrink finish performance, perforated line openability and thermal blocking re...
|