PURPOSE: To obtain a conductive ceramics expressed by the formula and having excellent corrosion resistance and mechanical strength by heating a mixture consisting of a nitrate and/or chloride of metal selected from In, Sc, Y, Tl and Ga and Cu at a prescribed temperature.
CONSTITUTION: A compound consisting of a nitrate and/or chloride of metal M selected from In, Sc, Y and Ga is prepared. A compound consisting of nitrate and/or chloride of Cu is prepared. Then these compounds are blended except combination of nitrate of the above-mentioned metal M with Cu nitrate and chloride of the above-mentioned metal M and Cu chloride. The blend is heated at 200-600°C to provide the Cu oxide based conductive ceramics. The blend is heated at 200-600°C to provide the Cu oxide based conductive ceramics expressed by the formula (A is Cl or Cl and NO3; x+y=1 and x/y is 0-10; z is 0-8; w is 1-9).
TERADA NORIO
JO MASATOSHI
HIRABAYASHI MASAYUKI
SUGISE RIYOUJI
DAIMON HIROSHI
FUJII KAZUHIRO
UBE INDUSTRIES
Next Patent: FABRIC OF FLAT FILAMENT