To provide a low-cost machine member which has excellent erosion resistance, wear resistance and strength even if it has a shape hard to be coated with slurry.
As for the method of producing the corrosion resistant and wear resistant member, in the method of coating the surface of a steel member with a corrosion resistant and wear resistant alloy, slurry obtained by mixing the alloy of spherical grains produced by an atomizing method, and in which a grain size lies in 30≤χ≤150μm in a grain size distribution (grain size width) of 1/3χto χμm, a resin as a binder and a solvent is dried and crushed to obtain raw material powder P; and the raw material powder P is stuck to the surface of a base material T made of steel heated to 100 to 400°C at which the resin in the raw material powder P can be fused; and thereafter, degreasing and sintering are performed.