Title:
ENVIRONMENT-FRIENDLY EXPERIMENT TABLE CERAMIC PANEL AND PREPARATION METHOD THEREFOR
Document Type and Number:
WIPO Patent Application WO/2020/052350
Kind Code:
A1
Abstract:
An environment-friendly experiment table ceramic panel, comprising a green body and a glaze surface. The green body comprises, in weight percent, raw materials of 20-30% of clay, 15-35% of low-temperature stone powder, 5-10% of high-temperature sand, 5-20% of bauxite, and 20-50% of ceramic waste brick recovery materials, wherein chemical components of the ceramic waste brick recovery materials comprise, in weight percent, 70-73% of SiO2, 17-20% of Al2O3, 0.5-1.0% of Fe2O3 + TiO2, 1.5-2.5% of CaO+MgO, and 5-6% of K2O + Na2O, and the ignition loss is lower than 1.0%.
More Like This:
Inventors:
KE SHANJUN (CN)
MA CHAO (CN)
MENG ZHENMING (CN)
MA CHAO (CN)
MENG ZHENMING (CN)
Application Number:
PCT/CN2019/097421
Publication Date:
March 19, 2020
Filing Date:
July 24, 2019
Export Citation:
Assignee:
FOSHAN OCEANO CERAM CO LTD (CN)
International Classes:
C04B33/24; B01L9/02; C04B35/64
Foreign References:
CN108706961A | 2018-10-26 | |||
CN106220134A | 2016-12-14 | |||
CN200948423Y | 2007-09-19 | |||
CN106220144A | 2016-12-14 | |||
JPS63307169A | 1988-12-14 | |||
DE2751897A1 | 1979-05-23 |
Attorney, Agent or Firm:
CHOFN INTELLECTUAL PROPERTY (CN)
Download PDF:
Previous Patent: FGFR INHIBITOR, PREPARATION METHOD THEREFOR AND APPLICATION THEREOF
Next Patent: HORIZONTAL DIRECTIONAL DRILLING RIG
Next Patent: HORIZONTAL DIRECTIONAL DRILLING RIG