ALUMINIUM ALLOY FIN MATERIAL FOR HEAT EXCHANGER EXCELLENT IN STRENGTH AND CORROSION RESISTANCE AFTER BRAZING
Document Type and Number:
Japanese Patent JP2013040367
Kind Code:
A
Abstract:

To provide an aluminium alloy fin material for a heat exchanger excellent in brazing property and strength after brazing and also excellent in intergranular corrosion resistance property.

This aluminium alloy fin material includes 1.0-2.0 mass% Mn, 0.5-1.3 mass% Si, 0.1-0.8 mass% Fe, over 0.20 mass% to 0.4 mass% Cu, 1.1 mass% to less than 2.0 mass% Zn, and the balance being Al and inevitable impurities. This aluminium alloy fin material excellent in the strength after brazing and corrosion resistance is characterized in that a matrix of the aluminium alloy fin material has a recrystallized structure.


Inventors:
OZAKI RYOTA
KOYAMA TAKAHIRO
Application Number:
JP2011177060A
Publication Date:
February 28, 2013
Filing Date:
August 12, 2011
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
SUMITOMO LIGHT METAL IND
International Classes:
C22C21/00
Domestic Patent References:
JP2002161323A2002-06-04
JP2010214378A2010-09-30
JP2007327118A2007-12-20
JP2002161324A2002-06-04
JPH0718358A1995-01-20
JPH0841573A1996-02-13
JP2012067385A2012-04-05
JP2002161324A2002-06-04
JPH0718358A1995-01-20
JPH0841573A1996-02-13
JP2012067385A2012-04-05
JP2002161323A2002-06-04
JP2010214378A2010-09-30
JP2007327118A2007-12-20
Other References:
JPN6015032380; 吉野路英: '自動車熱交換器用犠牲陽極フィン材の強度および耐食性に及ぼすSi,Cu添加の影響' 軽金属 Vol.59 No.5, 2009, P.229-235
JPN6015032380; 吉野路英: '自動車熱交換器用犠牲陽極フィン材の強度および耐食性に及ぼすSi,Cu添加の影響' 軽金属 Vol.59 No.5, 2009, P.229-235
Attorney, Agent or Firm:
Kenji Akatsuka
Yasuo Fukuda
Yasuyuki Sakata
Ken Shibuya