Abstract:
Provided is a method with which it is possible, when causing a sulfuration reaction to occur from a sulfuric acid acidic solution containing at least nickel through use of a sulfuration agent and generating a sulfide of nickel, to suitably control the grain size of the generated sulfide while maintaining high reaction efficiency. The sulfuration treatment method according to the present invention comprises supplying a sulfuric acid acidic solution that contains nickel to a reactor, adding hydrogen sulfide gas to the sulfuric acid acidic solution, and generating nickel sulfide, wherein unreacted gas among the hydrogen sulfide gas added to the sulfuric acid acidic solution is recovered, sodium hydroxide is added to the recovered hydrogen sulfide gas, sodium hydrosulfide is generated, and the resulting solution of sodium hydrosulfide is added to sulfuric acid acidic solution. At this time, when the sodium hydrosulfide solution is added, the grain size of the generated sulfide of nickel is set to 50 μm or higher by 50% particle size (D50) by controlling the amount of sodium hydrosulfide solution added to the reactor to which the sulfuric acid acidic solution is supplied.

Inventors:
FUKE TOMONAO (JP)
OISHI TAKAO (JP)
Application Number:
PCT/JP2017/003684
Publication Date:
August 17, 2017
Filing Date:
February 02, 2017
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
SUMITOMO METAL MINING CO (JP)
International Classes:
C22B23/00; C01G53/11; C22B3/08; C22B3/44
Domestic Patent References:
WO2015114913A12015-08-06
Foreign References:
JP2008156713A2008-07-10
Attorney, Agent or Firm:
SHOBAYASHI, Masayuki et al. (JP)
Download PDF: